项目
Properties |
单位
Unit |
测试方法
Tost Method |
机用膜
Machine Wrap Film |
手工膜
Hand Wrap Film |
比重
Spectific gravity |
g/cm3 |
ASTMD 1505 |
0.197 |
0.197 |
拉伸强度MD
Tensite strength at break TD |
Kg/cm2 |
ASTMD 885 |
≥380
≥250 |
≥300
≥200 |
断裂伸裂长率MD
Elongation at break TD |
% |
ASTMD882 |
≥400
≥700 |
≥350
≥600 |
直解撕裂强度MD
Rightangle tear strength TD |
N/mm |
HT |
≥75
≤90 |
≥75
≥90 |
粘性
Adhesion |
N/cm2 |
HT |
≥0.8 |
≥0.8 |
雾度
Haze |
% |
ASTMD1003 |
≤2 |
≤2 |