牌号
|
GB国标
|
C
|
Si
|
Mn
|
Cr
|
W
|
Fe
|
Co
|
堆焊层硬度
|
D802
|
EDCoCr-A-03
|
0.7-1.4
|
≤ 2
|
≤ 2
|
25-32
|
8-6
|
≤ 5
|
余量
|
HRC≥45
|
D812
|
EDCoCr-B-03
|
1.0-1.7
|
≤ 2
|
≤ 2
|
25-32
|
7-10
|
≤ 5
|
余量
|
HRC≥50
|
D822
|
EDCoCr-C-03
|
1.75-3.0
|
≤ 2
|
≤ 2
|
25-33
|
11-19
|
≤ 5
|
余量
|
HRC≥55
|
D842
|
EDCoCr-D-03
|
0.2-0.5
|
≤ 2
|
≤ 2
|
23-32
|
≤ 9.5
|
≤ 5
|
余量
|
HRC≥40-45
|
4、堆焊层须经粗磨,如发现缺陷时,按上述步骤进行焊补及缓冷。
|