Grade : | X3CrNiCu18-9-4建筑用耐腐蚀钢棒材 | |||||||
Number: | 1.4567 | |||||||
Classification: | 奥氏体不锈钢 | |||||||
Density: | 7.9 g/cm ³ | |||||||
Standard: | ||||||||
EN 10088-3:2005不锈钢。一般用途耐腐蚀钢的半成品、棒材、线材、型材和光亮产品的交货技术条件 | ||||||||
EN 10269:1999具有规定高温和/或低温性能的紧固件用钢和镍合金 | ||||||||
EN 10263-5:2001冷镦和冷挤压用钢条、棒材和线材。不锈钢交货技术条件 | ||||||||
EN 10088-1:2005不锈钢。不锈钢清单 | ||||||||
EN 10088-5:2009不锈钢。建筑用耐腐蚀钢棒材、棒材、线材、型材和光亮产品的交货技术条件 | ||||||||
Equivalent grades: | ||||||||
Chemical comb % of steel X3CrNiCu18-9-4 (1.4567): EN 10088-3-2005 | ||||||||
C | Si | Mn | Ni | P | S | Cr | N | Cu |
max 0.04 | max 1 | max 2 | 8.5 - 10.5 | max 0.045 | max 0.03 | 17 - 19 | max 0.11 | 3月4日 |
Mechanical properties of steel X3CrNiCu18-9-4 (1.4567) | ||||||||
Rm - Tensile strength (MPa) (+A) | 450-650 | |||||||
Rm - Tensile strength (MPa) (+AT+C) | 700-740 | |||||||
Rp0.2 0.2% proof strength (MPa) (+A) | 175 | |||||||
A - Min. elongation at fracture (%) (+A) | 45 | |||||||
Nominal diameter (mm): | 2 - 50 | |||||||
Z - Reduction in cross section on fracture (%) | 63-68 | |||||||
Brinell hardness (HB): (+A) | 215 | |||||||