首先将被保温物表面重垢除去,直接加水浸泡涂料1-2小时,并不断翻和成膏状物。施工时采用直涂法,将该品经纬交叉轻涂轻抹。首次涂层厚度不宜超过5mm,干后再涂第二层涂层厚度10-15mm,直至达到保温层厚度,待表面稍凝后压光,养护处理即可 http://guge6.qy6.com